Investigation of dynamic Jahn-Teller fluctuations in Ni3+-rich Li ion battery cathode materials

Dr Sian Dutton;Professor Aron Walsh;Miss Paromita Mukherjee;Dr David Voneshen;Mrs Nicola Kelly;Mr Liam Nagle-Cocco;Dr Hui Yang

Description

LiNi0.8Mn0.1Co0.1O2 , LiNi0.6Mn0.2Co0.2O2 and LiNi0.8Co0.15Al0.05O2, commonly known as Li NMC 811, Li NMC 622 and Li NCA respectively, are next-generation Li ion battery cathode materials containing Jahn-Teller active Ni3+ as the main redox-active ion. The presence of dynamic Jahn-Teller distortions, which would significantly impact their electrochemical performance, remains an open question. We propose to study the temperature evolution of the phonon modes associated with the dynamic Jahn-Teller distortions at two incident energies for Li NMC 811, Li NMC 622 and Li NCA.

Citations (0)

Mentions (0)

Metrics

Dataset Index

0.4

FAIR Score

73%

Citations

0

Mentions

0

Metrics Over Time

Publication Details

DOI

Publisher

ISIS Facility

Assigned Domain

Subfield

Organic Chemistry

Field

Chemistry

Domain

Physical Sciences

Confidence Score

33%

Source

Scholar Data Model

Keywords

STFC ISIS Neutron and Muon Data

Normalization Factors

FT

59.62

CTw

1.00

MTw

1.00