Published on 01 January 2021

Light intensity in reflection mode of PAAO (1st sample 2nd anodization)

View Dataset
Jurkevičiūtė, Aušrinė;Dutovs, Aleksandrs;Poplausks, Raimonds;Prikulis, Juris

Description

Light intensity data recorded during the anodization of aluminum polycrystal. Light source: SLS201L/M (ThorLabs). Spectrometer: USB4000 (OceanOptics). Spectra acquisition software: SpectraSuite (OceanOptics). Integration time: 340 us. Scans to average: 5. Spectrum is recorded every 50 ms during anodization. ref.txt includes reference spectra just before the start of anodization process. Anodization was performed in 0.3 mol/L oxalic acid at 40 V for 6 min.

Citations (0)

Mentions (0)

Metrics

Dataset Index

0.3

FAIR Score

13%

Citations

0

Mentions

0

Metrics Over Time

Publication Details

DOI

Publisher

Zenodo

Assigned Domain

Subfield

Bioengineering

Field

Chemical Engineering

Domain

Physical Sciences

Confidence Score

94%

Source

Open Alex

Keywords

spectroscopyanodizationtime dependentreflectionPAAO

Normalization Factors

FT

15.38

CTw

1.00

MTw

1.00